Mitsui Fybrel® E 400 Polyolefin Synthetic Pulp, Wet Processes
Subcategory: Polyethylene; Polyolefin
Material Notes: Fybrel® (Polyolefin Synthetic Pulp), a Mitsui Chemicals Inc. novel creation, is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type Y that is made from polypropylene. All are available in various grades in wet-lap (sheet) form. Applications: - Battery separators
- Disposable food trays and packaging
- Embossed paper and stationary (greeting cards)
- Filter elements for filtration systems
- Heat sealing paper for packaging
- Heat sealing tea bag paper
- Padding materials for automobiles and beds
- Replacement for asbestos in paint and roofing tiles
Information provided by Mitsui.
| Available Properties |
- Density
- Melting Point
- Moisture Content
- Canadian Standard Freeness
- Classified Fiber Length
- Drainage Factor
- Fiber Diameter
- Standard Weight
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|