Mitsui Fybrel® ESS-5 Polyolefin Synthetic Pulp, Dry Processes

 

Subcategory: Polyethylene; Polyolefin

Material Notes:
Fybrel® (Polyolefin Synthetic Pulp), a Mitsui Chemicals Inc. novel creation, is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type Y that is made from polypropylene. All are available in various grades in wet-lap (sheet) form.

Applications:

  • Battery separators
  • Disposable food trays and packaging
  • Embossed paper and stationary (greeting cards)
  • Filter elements for filtration systems
  • Heat sealing paper for packaging
  • Heat sealing tea bag paper
  • Padding materials for automobiles and beds
  • Replacement for asbestos in paint and roofing tiles

Information provided by Mitsui.

Available Properties
  • Density
  • Melting Point
  • Moisture Content
  • Classified Fiber Length
  • Fiber Diameter
  • Standard Weight
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。