Mitsui Chemicals UNISTOLE™ R-200X Modified Polyolefin
Subcategory: Polyolefin; Thermoplastic
Material Notes: UNISTOLE™ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent.
Characteristics - Excellent adhesion to various metals
- Exceptional heat resistance and heat resistant adhesion
- Superb resistance to retort treatment
- Useable with simple equipment such as gravure coaters, roll coaters and sprays
- UNISTOLE™ R contains no chlorine
Applications - Adhesive for bonding metal foil and a polyolefin such as aluminum foil and PP film to make retort packages, PTP packages, easy peal packages, etc.
- Metal coating agent (bonding of metal by extruding PP onto it, automotive parts, etc.)
- Modifier when added to paints, adhesives, printing inks, since it improves adhesion to PP
Information provided by Mitsui Chemicals America, Inc.
| Available Properties |
- Particle Size
- Viscosity
- Viscosity Measurement
- Collected Volatile Condensable Material
- Remarks
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|