Mitsui Chemicals EXCEREX™ 40800(T), Functional Olefin Oligomer
Subcategory: Additive/Filler for Polymer
Material Notes: EXCEREX™ is an innovative processing improvement agent created with metallocene catalysis technology. EXCEREX™ gains in a number of ares simultaneously, including faster processing speeds, lower resin temperatures, reduced scorching, and reduced changeover times.Information provided by Mitsui Chemicals
| Available Properties |
- Density
- Molecular Weight
- Melting Point
- Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|