ITW Plexus™ MA920 Methacrylate Adhesive
Subcategory: Methacrylate; Adhesive; Thermoset
Material Notes: Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies. All purpose, low odor, short open time. Information provided by Illinois Tool Works.
| Available Properties |
- Density
- Viscosity
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Shear Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Pot Life
- Color
- Fixture Time
- Gap Filling
- Mix Ratio
|
|
|
|
| Property Data |