ITW Plexus™ AO420FS Methacrylate Adhesive
Subcategory: Methacrylate; Adhesive; Thermoset
Material Notes: Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Shear Strength
- Maximum Service Temperature, Air
|
|
|
|