Material Notes: The temperature control setting is 4 and the flash point is 536°F (280°C). The auto ignition is 626°F (330°C). The ball and ring soft point is 305°F (152°C); ASTM E-28-6-7. The peal strength on canvas is 15 PIW at 72°F (22°C). The bonding range of a 1/8 inch bead on Douglas Fir to Douglas Fir is 30 seconds. The delivery rate is 65 seconds for 1 inch x 3 inch cartridge. Self-extinguishing version of 3748 Adhesive meets UL 94 V-O, UL 1410 requirements. Information provided by 3M Adhesives Division.
| Available Properties |
- Brookfield Viscosity
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Impact Test
- Impact Test
- Maximum Service Temperature, Air
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|