3M Jet-melt™ Adhesive: High-Melt Technology 3783 Brown
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: The flash point is 480°F (249°C). The auto ignition is 827°F (442°C). The ball and ring soft point is 190°F (88°C); ASTM E-28-6-7. The peal strength on canvas is 22 PIW at 72°F (22°C). The bonding range of a 1/8 inch bead on Douglas Fir to Douglas Fir is 45 seconds. The delivery rate is 60 seconds for 1 inch x 3 inch cartridge. The ingredients of the product when dried after application are listed as indirect food additives under FDA regulation 21 CFR 175.105. Multi-purpose with good heat and impact resistance. Can bond many plastics and light gauge metals. Information provided by 3M Adhesives Division.
| Available Properties |
- Brookfield Viscosity
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Impact Test
- Impact Test
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|