3M Scotch-Weld™ Two-Part Epoxy Adhesive 2216 B/A Gray
Subcategory: Epoxy; Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Two-part, room-temperature or heat curing epoxy adhesives provide high-strength bonds on a wide variety of substrates. Bond is often stronger than the parts being bonded. Features include long worklife adhesive, rigid epoxy, 8-12 hours handling strength, and can bond plastic, metal and other dissimilar materials. Mix ratio by volume 2:3. Average T-Peel at 75°F (24°C) is 25 PIW; 180° peel tested on 0.030 inch aluminum per ASTM D 1876-61T. Information provided by 3M Adhesives Division.
| Available Properties |
- Brookfield Viscosity
- Shear Strength
- Processing Temperature
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|