3M Scotch-Weld™ Two-Part Urethane Adhesive 3535 B/A Off-white
Subcategory: Adhesive; Polyurethane, TS; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Two-part urethane adhesives cure at room temperature or with heat to provide tough, impact resistant bonds with high peel strength. Features include fast cure adhesive, 15-20 minutes handling strength, semi-rigid urethane, and faster setting version of 3532 B/A Adhesive. Mix ratio by volume 1:1. Average T-Peel at 75°F (24°C) is 25 PIW; 180° peel tested on 0.030 inch aluminum per ASTM D 1876-61T. Information provided by 3M Adhesives Division.
| Available Properties |
- Brookfield Viscosity
- Shear Strength
- Processing Temperature
- Pot Life
|
|
|
|
| Property Data |