3M Scotch-Weld™ Adhesive in Duo-Pak Cartridges DP-190 Gray
Subcategory: Epoxy; Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Features include long worklife adhesive, flexible epoxy, 8-12 hours handling strength, and can bond metals, plastics and many other dissimilar materials. Mix ratio by volume 1:1. Average T-Peel at 75°F (24°C) is 20 PIW; 180° peel tested on 0.030 inch aluminum per ASTM D 1876-61T. General info on Scotch-Weld™ Duo-Pak cartridges: Two-part room-temperature curing epoxy, urethane and acrylic adhesives especially formulated and packaged for use in the EPX Applicator. Information provided by 3M Adhesives Division.
| Available Properties |
- Brookfield Viscosity
- Shear Strength
- Processing Temperature
- Pot Life
|
|
|
|