3M Scotch-Weld™ One-Part Epoxy Adhesive 1469 Cream
Subcategory: Epoxy; Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: One part epoxy adhesive is a structural strength product that eliminates the mixing and weighing of two-part systems. This product must be heat cured. A 350°F (177°C) curing epoxy with excellent performance at elevated temperatures. Meets requirements of MMM-A-132 Type III, Class 3, Group 4 Optimum cure takes 120 minutes at 177°C/350°F, 10 psi. Average T-Peel at 75°F (24°C) is 2 PIW; 180° peel tested on aluminum per ASTM D 1876-61T. Information provided by 3M Adhesives Division.
| Available Properties |
- Viscosity
- Shear Strength
- Processing Temperature
|
|
|
|