3M Scotch-Weld™ One-Part Epoxy Adhesive 2214 Hi-Temp New Formula Gray
Subcategory: Epoxy; Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: One part epoxy adhesive is a structural strength product that eliminates the mixing and weighing of two-part systems. This product must be heat cured. Adhesive with exceptional performance at elevated temperatures and excellent performance under high temperature high humidity conditions. Resists attack by hot ethylene glycol. Viscosity is paste. Optimum cure takes 60 minutes at 121°C/250°F, 10 psi. Average T-Peel at 75°F (24°C) is 5 PIW; 180° peel tested on aluminum per ASTM D 1876-61T. Information provided by 3M Adhesives Division.