3M Scotch-Weld™ One-Part Epoxy Adhesive 2214 Non-metallic filled Cream
Subcategory: Epoxy; Adhesive; Thermoset; Polymer
Key Words: 3M Adhesives Division
Material Notes: One part epoxy adhesive is a structural strength product that eliminates the mixing and weighing of two-part systems. This product must be heat cured. A cream colored non-metallic version of 2214 Regular Adhesive suggested for electrical applications where insulating qualities are desired. Viscosity is paste. Optimum cure takes 60 minutes at 121°C/250°F, 10 psi. Average T-Peel at 75°F (24°C) is 7 PIW; 180° peel tested on aluminum per ASTM D 1876-61T. Information provided by 3M Adhesives Division.
| Available Properties |
- Shear Strength
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|