3M Scotch-Weld™ Metal Primer 1945 B/A Green
Subcategory: Epoxy; Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Metal primer that can be used to help improve adhesion and provide better environmental resistance when used with Scotch-Weld Adhesives. It is a two-part chemically curing, corrosion resistant primer to improve adhesion of urethanes and epoxies to many metals as well as offering increased corrosion protection. It cures at room temperature and has excellent adhesion to many metals. Features include 1:1 mix ratio two-part epoxy primer, 8 hour potlife, and brush, spray or dip application. Information provided by 3M Adhesives Division.
| Available Properties |
- Viscosity
- Processing Temperature
|
|
|
|