3M Aerosol Super 74 Foam Fast Adhesive
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Fast tack with foam-tearing strength and soft non-dimpling glue line. General upholstery foam bonding. Plus knife edge bonding, boxing, edge turning. Spray width 1"-3" variable. Bonding range surfaces: one side not recommended, both sides 15 minutes. Peel strength is 20 PIW; ITSD T.M. C-449. Temperature resistance is 120°F (49°C); ITSD T.M. C-483; 500 g load for 1 hour at noted temperature. Coverage is 260 square feet per 24 ounce container. Information provided by 3M Adhesives Division.
| Available Properties |
- Shear Strength
- Maximum Service Temperature, Air
- Processing Temperature
|
|
|
|