3M Aerosol 75 Repositionable Adhesive
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Clear "tape-like" adhesive holds badges during stitching and patterns prior to cutting. No bleed, stain or wrinkle. Spray width 1 1/2". Bonding range surfaces: one side 1 hour, both sides 3 hours. Peel strength is 5 PIW; ITSD T.M. C-449. Temperature resistance is 120°F (49°C); ITSD T.M. C-483; 500 g load for 1 hour at noted temperature. Coverage is 100 square feet per 16 ounce container. Information provided by 3M Adhesives Division.