3M Aerosol 80 Neoprene Contact Adhesive
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Neoprene-based contact adhesive with plasticizer resistance. Can bond supported vinyl, leather, and most rubber. Adheres to most plastics, laminate and wood. Resists over 200°F (93°C). Spray width 1"-2" varialbe. Bonding range surfaces: one side not recommended, both sides 1 hours. Peel strength is 35 PIW; ITSD T.M. C-449. Temperature resistance is 200°F (93°C); ITSD T.M. C-483; 500 g load for 1 hour at noted temperature. Coverage is 75 square feet per 24 ounce container. Information provided by 3M Adhesives Division.
| Available Properties |
- Shear Strength
- Maximum Service Temperature, Air
- Processing Temperature
|
|
|
|