3M Shipping-Mate Packaging Aerosol Labeling Adhesive
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Clear, fast-tacking. Holds labels to many corrugated cartons and problem surfaces such as glass, plastic and more. Moisture-resistant bond. Spray width 2 1/2". Bonding range surfaces: one side 10 minunutes, both sides not recommended. Temperature resistance is 136°F (54°C); ITSD T.M. C-483; 500 g load for 1 hour at noted temperature. Coverage is 90 square feet per 24 ounce container. Information provided by 3M Adhesives Division.
| Available Properties |
- Shear Strength
- Processing Temperature
|
|
|
|
| Property Data |