3M Fastbond™ Water-based Adhesive 2000-NF Blue Adhesive (with spray Activator #1)
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: An adhesive that offers low or not VOCs (Volatile Organic compounds) and nonflammability (in the wet state) to bond a wide variety of substrates. Water-dispersed, activated adhesive which provides immediate bonding and handling strength without forced drying. The solids weight is approximately 49%. The color is blue, the consistency is thin liquid, and the application method is co-spray. The bond range holds up to 2 hours. Peel strength is 4.1 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate. Information provided by 3M Adhesives Division.
|
|
|