3M Scotch-Grip™/Fastbond™ Water-based Adhesive 4224-NF Clear Industrial Adhesive
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: An adhesive that offers low or not VOCs (Volatile Organic compounds) and nonflammability (in the wet state) to bond a wide variety of substrates. Permanently pressure sensitive with aggressive tack. Plasticizer resistant. Low VOC content. The solids weight is approximately 40%. The color is clear, the consistency is thick liquid, and the application method is spray, brush, roller, trowel, roll coat, or knife coat. The bond range holds 30 days plus. Peel strength is 4.4 PIW at 75°F (24°C); primed polyester to steel at 2 inches/minutes separation rate. Information provided by 3M Adhesives Division.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|