3M Scotch-Grip™/Fastbond™ Water-based Adhesive 4268-NF Industrial Adhesive
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: An adhesive that offers low or not VOCs (Volatile Organic compounds) and nonflammability (in the wet state) to bond a wide variety of substrates. High-coverage pressure-sensitive adhesive with repositionability. Low VOC content and low odor. The solids weight is approximately 48%. The color is clear, the consistency is medium liquid, and the application method is spray, brush, roller, trowel, roll coat, or knife coat. The bond range holds 30 days plus. Peel strength is 6.3 PIW at 75°F (24°C); primed polyester to steel at 2 inches/minutes separation rate. Information provided by 3M Adhesives Division.
|
|
|