3M Scotch-Grip™/Fastbond™ High Performance Contact Adhesive 1357-L
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: An adhesive with years of successful history in a wide range of industrial product assembly applications. Lower solids, lower viscosity version of 1357 Adhesive for automatic spray applications. The solids weight is approximately 18%. The flash point is -14°F/-26°C. The color is gray-green, the consistency is thin liquid, and the application method is spray. The bond range holds for a 30 minute minimum. Peel strength is 42 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate. Information provided by 3M Adhesives Division.
| Available Properties |
- Shear Strength
- Processing Temperature
|
|
|
|
| Property Data |