3M Scotch-Grip™ Rubber and Gasket Adhesive 847
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: A high strength adhesive used throughout industry to bond many rubber and gasket materials to themselves and to other substrates. Quick drying and flexible with fuel and oil resistance. Heat and solvent reactivatable. Curable with heat. The solids weight is approximately 36%. The flash point is 0°F/-18°C. The color is brown, the consistency is medium liquid, and the application method is brush or flow. The bond range holds up to 15 minutes. Peel strength is 40 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate. Information provided by 3M Adhesives Division.
|
|
|