Material Notes: A high strength adhesive used throughout industry to bond many rubber and gasket materials to themselves and to other substrates. Higher viscosity version of 847 Adhesive. The solids weight is approximately 50%. The flash point is 0°F/-18°C. The color is brown, the consistency is thick liquid, and the application method is brush or flow. The bond range holds up to 10 minutes. Peel strength is 40 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate. Information provided by 3M Adhesives Division.
|
|
|