3M Scotch-Grip™ and Fastbond 1870 Industrial Adhesive
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications. Single surface application with very long tack range. Resists bleed through. Flexible bond. The solids weight is approximately 26%. The flash point is -7°F/-22°C. The color is tan, the consistency is thin liquid, and the application method is spray or brush. The bond range holds up to 40 minutes. Peel strength is 7 PIW at 75°F (24°C); maple to itself at 50% R.H. Test at 0.1 inches/min. separation rate. Information provided by 3M Adhesives Division.
|
|
|