3M Scotch-Grip™ and Fastbond 4799 Industrial Adhesive
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications. Brushable paste consistency with low soak-in on porous surfaces. Can bond EPDM rubber. The solids weight is approximately 36%. The flash point is -14°F/-26°C. The color is black, the consistency is thin liquid, and the application method is brush trowel. The bond range holds up to 15 minutes. Peel strength is 28 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate. Information provided by 3M Adhesives Division.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|