3M Scotch-Grip™ Plastic Adhesive 1099
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: A high strength fast-drying adhesive with unique plastic bonding capabilities for a wide variety of industries. Fast drying and heat curable. Resists weathering, water, oil, plasticizer migration, aliphatic fuels. Meets MIL-A-189C, Class 2. The solids weight is approximately 32%. The flash point is 0°F/-18°C. The color is light tan, the consistency is medium liquid, and the application method is brush or flow . The bond range holds up to 40 minutes. Peel strength is 31 PIW at 75°F (24°C); canvas to cold rolled steel at 2 inches/minute separation rate. Information provided by 3M Adhesives Division.