3M Scotch-Seal™/Weatherban™ 606-NF Sealant
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Smooth handling, weather resistant sealant for metal, wood, painted or primed surfaces and certain adraded plastics. Skins over in 20-40 minutes with low shrinkage. Permits weld-through and painting. The solids weight is approximately 78%. The color is white, the consistency is pumpable paste, and the application method is hand or pressure caulk. Cure or dry time 7 days (1/4" dia. Bead). Information provided by 3M Adhesives Division.
| Available Properties |
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|
| Property Data |