3M Scotch-Seal™/Weatherban™ 800 Sealant
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Air dries to a flexible, rubbery seal for aluminum, cold rolled steel, glass, many plastics and other surfaces. Resists weather, water, oils, fuel, detergent and soap solutions. The solids weight is approximately 51.5%. The flash point is 20°F/-7°C. The color is reddish brown, the consistency is heavy liquid, and the application method is brush or flow. Cure or dry time 1-3 days. Information provided by 3M Adhesives Division.
| Available Properties |
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|