3M Scotch-Seal™/Weatherban™ 900 Sealant
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Firm, rubbery seal with gap filling properties for aluminum, galvanized steel, cold rolled steel and more. Economically seals medium and high pressure heating and air conditioning ducts. The solids weight is approximately 66%. The flash point is 1°F/-17°C. The color is gray, the consistency is mastic, and the application method is hand or pressure caulk. Cure or dry time 1-2 days. Information provided by 3M Adhesives Division.