3M Scotch-Seal™/Weatherban™ 5200 Sealant
Subcategory: Adhesive; Thermoset
Key Words: 3M Adhesives Division
Material Notes: Rubbery, extremely strong sealant/adhesive for mahogany, teak, cedar, fir, plywood and fiberglass. Nonshrinking, one part moisture cure. Resists weather, fresh and salt water. The solids weight is approximately 99%. The flash point is greater than 150°F/greater than 66°C. The color is white, mahogany or tan, the consistency is thixotropic liquid, and the application method is hand or pressure caulk. Cure or dry time 7 days (1/4" dia. bead). Information provided by 3M Adhesives Division.
| Available Properties |
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
|
|
|
|