Montell 6323 Polypropylene Homopolymer, Easy Molding
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: General Purpose Key Features: easy molding, FDA acceptable, general purpose polypropylene homopolymer resin Applications: containers, closures, hospital and institutional ware, toys Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: Pro-fax 6323 resin is a general purpose polypropylene homopolymer. It meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. It has a UL yellow card RTI. These UL ratings apply only to natural color resin. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|