Montell 6331NW Polypropylene Homopolymer, Nucleated/Antistat
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: antistatic and nucleated polypropylene homopolymer resin, short cycle time, resists dust pickup, low odor Applications: lightweight containers, closures, hospital and institutional ware, toys Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: Pro-fax 6331NW polypropylene homopolymer resin is nucleated for faster crystallization and features antistatic properties. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. It has a UL yellow card RTI, which apply to all colors. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|