Montell KY 6100 Polypropylene Homopolymer, General Purpose
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Extrusion Key Features: general purpose polypropylene homopolymer resin for extrusion, FDA acceptable, high tensile strength, easily oriented to achieve balanced high strength products Applications: carpet backing, ropes and twines Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: KY 6100, a general purpose polypropylene homopolymer resin, is suitable for general extrusion and film fiber applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications, It has a UL yellow card resin, which applies only to the natural color resin. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|