Montell PD191 Polypropylene Homopolymer, Fractional Melt Flow
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: fractional melt flow polypropylene homopolymer resin, stiff, good heat-age life, high resistance to solvents, FDA acceptable Applications: strapping Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: Pro-fax PD191 fractional melt flow polypropylene homopolymer resin is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|