Montell PDC1194 Polypropylene Homopolymer, High Flow
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Injection Molding Key Features: high flow polypropylene homopolymer resin for injection molding, FDA acceptable, ease of processing allows increased design freedom, excellent dimensional stability, processes with low built-in stress, improved room temperature toughness for molded parts Applications: compounding, extrusion applications, thin complex parts Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: PDC1194, an easily processed, high flow, controlled rheology polypropylene homopolymer resin, is designed for injection molding or extrusion applications. It is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|