Montell PF633 Polypropylene Homopolymer, High Melt Strength

 

Subcategory: Polypropylene; Thermoplastic

Close Analogs:

Basell is the successor company to Montell.

Material Notes:
Primary Processing Method: Additive for Extrusion

Key Features: high melt strength polypropylene homopolymer resin, FDA acceptable, high draw ratios, reduced check-in, contributes to bubble stability in blown film, good moisture barrier properties, good chemical and grease resistance, low odor and taste transfer

Applications: blown film, extrusion coating

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: Pro-fax PF633 high melt strength polypropylene homopolymer resin is used as an additive for extrusion applications. It can improve extrusion processability by increasing melt curtain stability. This results in more uniform draw at higher rates. As a blend component, it can impart higher service temperature and higher stiffness. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Rockwell R
  • Tensile Strength, Yield
  • Elongation at Yield
  • Flexural Modulus
  • Deflection Temperature at 0.46 MPa (66 psi)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。