Montell SM 6100 Polypropylene Homopolymer, High Melt Flow
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Injection Molding Key Features: polypropylene homopolymer resin for injection molding, FDA acceptable, high flow permits filling of multi-cavity molds, good stiffness good long-term heat stability, low odor and taste transfer Applications: medical ware, packaging, containers Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: SM 6100, a high melt flow polypropylene homopolymer resin, is suitable for general injection molding applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|