Montell SS 6100 Polypropylene Homopolymer, Multi-Filament Extrusion
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: polypropylene homopolymer resin for multi-filament extrusion, excellent processing stability, high tensile strength, uniform consistent lots, FDA acceptable Applications: melt spun fibers Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: SS 6100, a high melt flow polypropylene homopolymer resin, is designed for melt-filament extrusion applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|