Montell SA861 Polypropylene Random Copolymer, Cast Film Extrusion
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: polypropylene random copolymer resin formulated for cast film extrusion, good optical properties, excellent slip properties, FDA acceptable, improved cold temperature impact resistance Applications: bags for hosiery, packaging for produce, sheet protectors, photograph pockets, card display sleeves Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: Pro-fax SA861 polypropylene random copolymer resin, formulated with slip and antilock, is designed for cast film packaging applications. Cast film made with this resin has exceptional clarity and gloss, as well as improved cold temperature impact resistance and broader heat seal range compared to homopolymer polypropylene. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Secant Modulus, MD
- Secant Modulus, TD
- Izod Impact, Notched
- Coefficient of Friction
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Deflection Temperature at 0.46 MPa (66 psi)
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|