Montell 7523 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Injection Molding Key Features: good cold impact resistance, good stiffness and impact balance, excellent dimensional stability, FDA acceptable Applications: seating, appliances, automotive parts, housewares Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: Pro-fax 7523 medium impact polypropylene copolymer resin is designed for injection molding applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|