Montell 7624 Polypropylene Impact Copolymer, Heat- and Extraction-Resistant
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Injection Molding Key Features: resistant to aging at high temperatures in both wet and dry environments, good cold impact resistance, excellent dimensional stability, FDA acceptable, Applications: appliances, automotive under-the-hood appliances Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: Pro-fax 7624 medium impact polypropylene copolymer resin is highly resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of properties and is used for injection molding applications. It has a UL yellow card RTI, which applies to all colors. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|