Montell SB751 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: high flow, medium impact polypropylene copolymer resin, FDA acceptable, excellent dimensional stability, good stiffness, minimum warpage and wider design latitude Applications: chemical containers and lids, thin complex parts, shipping containers, thin walled cylinders Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: Pro-fax SB751 high melt flow, controlled rheology, medium impact polypropylene copolymer resin is designed for injection molding applications requiring an excellent balance of stiffness, impact resistance, and processability. It is available in pellet form. It has passed USP Class VI testing. It has a UL yellow card, which applies to all colors. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|