Montell SB786 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: blush-resistant, easy molding, high impact polypropylene copolymer resin, good cold impact resistance, good stiffness, FDA acceptable Applications: automotive battery case, housewares, closures Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications. Description: Pro-fax SB786 easy molding, blush-resistant, high impact polypropylene copolymer resin is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. It has a UL yellow card RTI, which applies to all colors. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- UL RTI, Mechanical with Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|