Montell SC917 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: high flow for ease of mold filling, minimum warpage and wider design latitude, nucleation also shortens cycles, higher productivity, resists dust and dirt pick-up, slip agent eases part ejection, good cold impact resistance, excellent gloss, good stiffness and impact balance, FDA acceptable Applications: dairy containers, margarine containers, cutlery, housewares Meets FDA requirements in 21 CFR 177.1520 for all food contact, excluding cooking applications. Description: Pro-fax SC917 fully formulated medium impact polypropylene copolymer resin is designed with a very high melt flow for thin wall injection molding applications. It exceeds the performance of competitive grades by offering a superior balance of stiffness, impact resistance, gloss and fast cycling properties. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|