Montell SE191 Polypropylene Impact Copolymer

 

Subcategory: Polypropylene; Thermoplastic

Close Analogs:

Basell is the successor company to Montell.

Material Notes:

Key Features: excellent electrical and physical properties, excellent resistance to environmental and thermal stress-cracking, low density an low dielectric constant contribute to light and smaller cables, tailored for high speed processing on thin-walled constructions

Applications: telephone singles general primary insulation

All ingredients meet TSCA (US) and DSL (Canada) registration requirements.

Description: Pro-fax SE191 low melt flow, electrical grade polypropylene copolymer resin has outstanding toughness, flex-life and abrasion resistance. This resin demonstrates good processing behavior and is tailored for trouble-free production of primary cable insulation, especially filled telephone cable because its unique stabilizer system resists extraction by petroleum-jelly based filling compounds. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

Available Properties
  • Density
  • Environmental Stress Crack Resistance
  • Melt Flow
  • Tensile Strength, Yield
  • Elongation at Yield
  • Flexural Modulus
  • Impact Test
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。