Montell SV954 Polypropylene Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes:
Key Features: nucleation shortens cycles for higher productivity, resists dirt and dust pick-up, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling and minimum warpage, low odor and taste transfer, FDA acceptable Applications: dairy containers, housewares and consumer products Meets FDA requirements in 21 CFR 177.1520 for all food contact, excluding cooking applications. Description: Pro-fax SV954 easy molding, fully formulated, high melt flow, medium impact polypropylene copolymer resin is designed for thin-wall applications requiring an excellent balance of stiffness and impact resistance. It is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|