Montell Adflex KS-021P TPO Resin

 

Subcategory: Thermoplastic

Close Analogs:

Basell is the successor company to Montell.

Material Notes:
Primary Processing Method: Blown Film/Impact Modification

Key Features: excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, FDA acceptable, no slip, no antiblock thermoplastic olefin resin

Applications: films, impact modification, toys, lawn and garden equipment

Meets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600.

Description: Adflex KS-021P thermoplastic olefin resin designed for impact modification of polypropylene, as well as monolayer and multilayer air quenched flown films (no slip, no anitblock). It is based monproprietary Montell process technology. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Izod Impact, Notched
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。