Montell Adflex KS-021P TPO Resin
Subcategory: Thermoplastic
Close Analogs: Basell is the successor company to Montell.
Material Notes: Primary Processing Method: Blown Film/Impact Modification Key Features: excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, FDA acceptable, no slip, no antiblock thermoplastic olefin resin Applications: films, impact modification, toys, lawn and garden equipment Meets FDA requirements in 21 CFR 177.2600 for rubber articles with repeated use applications. The final item is subject to extraction requirements in 21 CFR 177.2600. Description: Adflex KS-021P thermoplastic olefin resin designed for impact modification of polypropylene, as well as monolayer and multilayer air quenched flown films (no slip, no anitblock). It is based monproprietary Montell process technology. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for resins in rubber articles for repeated use applications. All ingredients meet the chemical registration requirements of TSCA and DSL. Information provided by Montell Polyolefins.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,